– Tensile Strength: 655 MPa
– Yield Strength: 275 MPa
– Elongation: 25%
– Hardness: 201 HB
Technical Properties:
– Density: 7.84 g/cm3
– Young’s Modulus: 210 GPa
– Poisson’s Ratio: 0.3
– Thermal Conductivity: 24 W/m*K
– Specific Heat Capacity: 502 J/kg*K
Chemical Composition:
– Carbon (C): 0.08%
– Manganese (Mn): 2%
– Silicon (Si): 0.75%
– Phosphorus (P): 0.04%
– Sulfur (S): 0.03%
– Chromium (Cr): 17%
– Nickel (Ni): 10%
– Molybdenum (Mo): 2%
[ad_2]