Technical properties:
– Tensile strength: 1100-1300 MPa
– Yield strength: 900-1000 MPa
– Elongation: 15-20%
– Hardness: 250-300 HB
Chemical composition:
– Carbon (C): 0.20-0.25%
– Manganese (Mn): 1.50% max
– Silicon (Si): 0.40% max
– Phosphorus (P): 0.010% max
– Sulfur (S): 0.010% max
– Chromium (Cr): 0.90-1.20%
– Molybdenum (Mo): 0.15-0.30%
Applications:
– Structural components in heavy machinery
– Load-bearing parts in construction and infrastructure
– Mining equipment
– Pressure vessels
– Automotive and aerospace components
Overall, the 425C11 steel grade offers a combination of high strength, good formability, and excellent weldability, making it a versatile and reliable material for a variety of industrial applications.