1. Tensile Strength: 650-850 MPa
2. Yield Strength: 450 MPa
3. Elongation: 20%
4. Hardness: 180-220 HB
Technical Properties of 405S17 Steel Grade:
1. Density: 7.75 g/cm3
2. Thermal Expansion: 10.5 x 10-6 /K
3. Thermal Conductivity: 25 W/m.K
4. Electrical Resistivity: 0.63 x10-6 Ω.m
Chemical Composition of 405S17 Steel Grade:
– Carbon (C): 0.08% max
– Silicon (Si): 1.00% max
– Manganese (Mn): 1.00% max
– Phosphorus (P): 0.040% max
– Sulfur (S): 0.030% max
– Chromium (Cr): 11.5-14.5%
– Nickel (Ni): 1.00% max
Maximizing Performance and Efficiency with 405S17 Steel Grade in Engineering Projects:
1. Utilize the high tensile strength and yield strength of 405S17 steel to design lightweight yet strong engineering components.
2. Take advantage of the good elongation and hardness of 405S17 steel to ensure durability and resistance to wear and tear in engineering applications.
3. Leverage the favorable technical properties such as thermal expansion and conductivity to optimize the performance and efficiency of heat transfer and mechanical stability in engineering projects.
4. Consider the specific chemical composition of 405S17 steel to meet the requirements of corrosion resistance, strength, and machinability in various engineering applications.
5. Employ advanced manufacturing techniques and processes to maximize the benefits of 405S17 steel grade in engineering projects, such as forming, welding, and heat treatment, to enhance properties and performance.