Mechanical Properties:
– Tensile strength: 900-1100 MPa
– Yield strength: 700-900 MPa
– Elongation: 12-16%
– Hardness: 270-330 HB
Technical Properties:
– Density: 7.85 g/cm3
– Thermal conductivity: 44.5 W/mK
– Specific heat capacity: 486 J/kgK
– Coefficient of thermal expansion: 11.1 x 10-6 K-1
Chemical Composition:
– Carbon (C): 0.14-0.19%
– Silicon (Si): 0.10-0.40%
– Manganese (Mn): 0.60-0.90%
– Phosphorus (P): 0.025% max
– Sulfur (S): 0.035% max
– Nickel (Ni): 1.40-1.70%
– Chromium (Cr): 1.00-1.30%
The combination of nickel and chromium in the chemical composition of 16NiCr11 steel provides good hardenability, wear resistance, and high fatigue strength. These properties make it suitable for use in high-stress applications where durability and longevity are critical.
Overall, the 16NiCr11 steel grade offers a good balance of mechanical properties, making it a popular choice for a wide range of mechanical components across various industries. Its high strength, good hardenability, and wear resistance make it a versatile and reliable material for demanding applications.