Mechanical properties:
– Tensile strength: 370-540 MPa
– Yield strength: 230-400 MPa
– Elongation: 25-28%
– Hardness: 60-80 HRB
Technical properties:
– Density: 7.85 g/cm3
– Young’s modulus: 200 GPa
– Poisson’s ratio: 0.30
– Thermal expansion: 11.0 x 10-6/K
Chemical composition:
– Carbon (C): 0.07-0.15%
– Manganese (Mn): 0.80-1.2%
– Phosphorus (P): 0.04% max
– Sulfur (S): 0.20-0.30%
– Silicon (Si): 0.10-0.40%
These properties make 240M07 steel grade suitable for applications where good machinability and moderate strength are required. It is often used in automotive, construction, and general engineering industries. However, it is important to consult with a materials engineer or steel supplier to determine the best heat treatment and machining practices for this steel grade.