– Tensile Strength: 1300 MPa
– Yield Strength: 1150 MPa
– Elongation at Break: 11%
– Hardness: 35 HRC
Technical Properties:
– Density: 7.85 g/cm3
– Thermal Conductivity: 52 W/m*K
– Electrical Conductivity: 5.9% IACS
Chemical Composition:
– Carbon: 0.25%
– Silicon: 1.0%
– Manganese: 1.5%
– Phosphorus: 0.04%
– Sulfur: 0.03%
– Chromium: 10.5%
– Nickel: 1.0%
– Molybdenum: 1.2%
– Vanadium: 0.2%
[ad_2]