Technical Properties:
– Tensile Strength: 900-1200 MPa
– Yield Strength: 650-900 MPa
– Elongation: 11-14%
– Hardness: 30-35 HRC
Chemical Composition:
– Carbon (C): 0.32-0.40%
– Silicon (Si): 0.40% max
– Manganese (Mn): 0.50-0.80%
– Phosphorus (P): 0.025% max
– Sulfur (S): 0.035% max
– Chromium (Cr): 0.90-1.20%
– Nickel (Ni): 0.90-1.20%
– Molybdenum (Mo): 0.15-0.30%
Applications:
36CrNiMo4 steel is commonly used in the manufacturing of gears, crankshafts, connecting rods, bolts, and other components that require high strength and toughness. It is also used in the automotive and machinery industry for applications that require high tensile and yield strength. Additionally, it is suitable for parts that require good wear resistance and high fatigue strength.