Mechanical properties:
– Tensile strength: 180 ksi
– Yield strength: 150 ksi
– Elongation: 14%
– Hardness: 28 HRC
Technical properties:
– Density: 7.85 g/cm3
– Melting point: 1420-1460°C
– Thermal conductivity: 51.9 W/mK
– Specific heat capacity: 473 J/kg·K
– Electrical resistivity: 0.55×10−6 Ω·m
Chemical composition:
– Carbon (C): 0.40-0.50%
– Manganese (Mn): 0.50-0.80%
– Silicon (Si): 0.20-0.35%
– Phosphorus (P): 0.035% max
– Sulfur (S): 0.035% max
– Chromium (Cr): 1.00-1.30%
– Nickel (Ni): 1.25-1.75%
– Molybdenum (Mo): 0.45-0.60%
This steel grade is often heat treated to achieve the desired mechanical properties. It can be welded using conventional welding methods with proper preheating and post-weld heat treatment. Overall, 425C11 is a versatile and reliable steel grade suitable for a wide range of industrial applications.