– Tensile Strength: 900-1100 MPa
– Yield Strength: 650-800 MPa
– Elongation: 14-16%
– Hardness: 250-300 HB
Technical Properties of 40NiCrMo22 Steel:
– Density: 7.85 g/cm3
– Thermal Conductivity: 45 W/(m*K)
– Specific Heat Capacity: 460 J/(kg*K)
– Young’s Modulus: 200 GPa
– Poisson’s Ratio: 0.3
Chemical Composition of 40NiCrMo22 Steel:
– Carbon (C): 0.37-0.45%
– Silicon (Si): 0.17-0.37%
– Manganese (Mn): 0.50-0.80%
– Phosphorus (P): ≤0.035%
– Sulfur (S): ≤0.035%
– Chromium (Cr): 0.80-1.10%
– Nickel (Ni): 1.65-2.00%
– Molybdenum (Mo): 0.15-0.25%