– Tensile strength: 530-800 MPa
– Yield strength: 260-420 MPa
– Elongation: 14-20%
– Hardness: 230-270 HB
Technical Properties of 230M07 Steel Grade:
– Good machinability
– Suitable for applications requiring high tensile strength and good wear resistance
– Can be heat treated to improve its mechanical properties
Chemical Composition of 230M07 Steel Grade:
– Carbon (C): 0.17-0.25%
– Silicon (Si): 0.10-0.35%
– Manganese (Mn): 0.60-0.90%
– Phosphorus (P): 0.040% max
– Sulfur (S): 0.040% max
– Chromium (Cr): 0.60-1.00%
– Nickel (Ni): 0.35% max
It is important to note that the specific chemical composition and mechanical properties of 230M07 steel may vary depending on the manufacturer and production process. Therefore, it is recommended to refer to the manufacturer’s datasheet for precise information.