– Tensile Strength: 770-950 MPa
– Yield Strength: 600-750 MPa
– Elongation: 13-16%
– Reduction in Area: 30-40%
– Impact Strength: 100-150 J
Technical properties of 14NiCr14 Steel Grade:
– Density: 7.85 g/cm³
– Melting point: 1420-1460°C
– Thermal conductivity: 43-49 W/m·K
– Specific heat capacity: 460-486 J/kg·K
– Electrical resistivity: 0.2-0.25 μΩ·m
Chemical composition of 14NiCr14 Steel Grade:
– Carbon (C): 0.10-0.17%
– Silicon (Si): 0.10-0.40%
– Manganese (Mn): 0.50-0.80%
– Phosphorus (P): 0.035% max
– Sulfur (S): 0.035% max
– Nickel (Ni): 1.40-1.70%
– Chromium (Cr): 1.30-1.70%